| 韓國科隆POM K300 K700 K900 |
|
性能項目
|
試驗條件[狀態]
|
測試方法
|
測試數據
|
數據單位
|
|
基本性能
|
吸水率
|
---
|
ASTM D-570
|
0.22
|
%
|
|
熔體流動速率
|
---
|
ASTM D-1238
|
9.0
|
g/10min
|
|
物理性能
|
比重
|
---
|
ASTM D-792
|
1.41
|
---
|
|
機械性能
|
拉伸強度
|
---
|
ASTM D-638
|
640
|
Kg/cm2
|
|
拉伸長率
|
---
|
ASTM D-638
|
65
|
%
|
|
彎曲強度
|
---
|
ASTM D-790
|
920
|
Kg/cm2
|
|
彎曲彈性率
|
---
|
ASTM D-790
|
26500
|
Kg/cm2
|
|
IZOD缺口衝擊強度
|
---
|
ASTM D-256
|
7.0
|
kg.cm/cm
|
|
洛氏硬度
|
---
|
ASTM D-785
|
80
|
Mscal
|
|
摩擦係數
|
---
|
ASTM D-1894
|
0.22
|
---
|
|
電氣性能
|
表面電阻係數
|
---
|
ASTM D-257
|
1×1016
|
Ω.cm
|
|
體積電阻係數
|
---
|
ASTM D-257
|
1×1014
|
Ω
|
|
絕緣破坏電壓
|
---
|
ASTM D-149
|
19
|
KV/mm
|
|
介電常數
|
---
|
ASTM D-150
|
3.7
|
---
|
|
介電損耗正切
|
---
|
ASTM D-150
|
0.006
|
---
|
|
耐ARC性
|
---
|
ASTM D-495
|
>200
|
sec
|
|
加工性能
|
成型收縮率
|
---
|
ASTM D-955
|
2.0
|
%
|
|
熱 性 能
|
熔點
|
---
|
ASTM D-1525
|
166
|
℃
|
|
熱變形溫度
|
4.6
|
---
|
160
|
Kg/cm2
|
|
熱變形溫度
|
18.6
|
ASTM D-648
|
110
|
℃
|
|
燃燒性
|
---
|
UL 94
|
HB
|
---
|
|
線膨脹係數
|
---
|
ASTM D-696
|
11-13
|
×10-5cm/cm/℃
|
|
|
|
|
|
|
|
|