| 韩国科隆POM K300 K700 K900 |
|
性能项目
|
试验条件[状态]
|
测试方法
|
测试数据
|
数据单位
|
|
基本性能
|
吸水率
|
---
|
ASTM D-570
|
0.22
|
%
|
|
熔体流动速率
|
---
|
ASTM D-1238
|
9.0
|
g/10min
|
|
物理性能
|
比重
|
---
|
ASTM D-792
|
1.41
|
---
|
|
机械性能
|
拉伸强度
|
---
|
ASTM D-638
|
640
|
Kg/cm2
|
|
拉伸长率
|
---
|
ASTM D-638
|
65
|
%
|
|
弯曲强度
|
---
|
ASTM D-790
|
920
|
Kg/cm2
|
|
弯曲弹性率
|
---
|
ASTM D-790
|
26500
|
Kg/cm2
|
|
IZOD缺口冲击强度
|
---
|
ASTM D-256
|
7.0
|
kg.cm/cm
|
|
洛氏硬度
|
---
|
ASTM D-785
|
80
|
Mscal
|
|
摩擦系数
|
---
|
ASTM D-1894
|
0.22
|
---
|
|
电气性能
|
表面电阻系数
|
---
|
ASTM D-257
|
1×1016
|
Ω.cm
|
|
体积电阻系数
|
---
|
ASTM D-257
|
1×1014
|
Ω
|
|
绝缘破坏电压
|
---
|
ASTM D-149
|
19
|
KV/mm
|
|
介电常数
|
---
|
ASTM D-150
|
3.7
|
---
|
|
介电损耗正切
|
---
|
ASTM D-150
|
0.006
|
---
|
|
耐ARC性
|
---
|
ASTM D-495
|
>200
|
sec
|
|
加工性能
|
成型收缩率
|
---
|
ASTM D-955
|
2.0
|
%
|
|
热 性 能
|
熔点
|
---
|
ASTM D-1525
|
166
|
℃
|
|
热变形温度
|
4.6
|
---
|
160
|
Kg/cm2
|
|
热变形温度
|
18.6
|
ASTM D-648
|
110
|
℃
|
|
燃烧性
|
---
|
UL 94
|
HB
|
---
|
|
线膨胀系数
|
---
|
ASTM D-696
|
11-13
|
×10-5cm/cm/℃
|
|
|
|
|
|
|
|
|